Compare / S355 vs SM520
S355 vs SM520
EN 10025-2:2019 · Steel
Europe's workhorse structural steel: 355 MPa minimum yield up to 16 mm, 470–630 MPa tensile from 3 to 100 mm.
Close matchMatches S355's yield (365 MPa ≤ 16 mm, 355 MPa 16–40 mm) with a higher tensile range, 520–640 MPa.
Mechanical
| Property | Condition | S355 | SM520 | Difference |
|---|---|---|---|---|
| Yield strength ReH | t = 16 mm | ≥ 355MPa3 | ≥ 365MPa1 | +2.8 % |
| t = 40 mm | ≥ 345MPa3 | ≥ 355MPa— | +2.9 % | |
| Tensile strength Rm | t = 3 mm | 510–680MPa3 | 520–640MPa2 | +2.0 % |
| t = 100 mm | 470–630MPa5 | 520–640MPa2 | +11 % | |
| t = 150 mm | 450–600MPa2 | 520–640MPa2 | +16 % | |
| t = 250 mm | 450–600MPa1 | 520–640MPa2 | +16 % | |
| t = 400 mm | 450–600MPa1 | 520–640MPa2 | +16 % |
Rows are matched by condition (thickness band, temperature, product form). A dash means the grade has no sourced value for that condition. Differences are SM520 relative to S355; for ranges the lower bound is compared.