Matipedia

Property class 10.9 / Equivalents

Is it really Property class 10.9? 1 “equivalents” checked

Cross-reference tables pair grades by name and history. Here each pairing is judged on the minimum values each standard guarantees, with the sources for both sides.

Close match

Same strength class; guaranteed values agree within a few MPa. Still check thickness bands and impact quality.

Approximate

Same class of steel, but at least one guaranteed value is lower or tested differently. Recheck the design.

    Not equivalent

    Commonly listed as an equivalent, but the guaranteed values do not support substitution.

      Side by side

      GradeStandardMin. yield at 10 mmTensile at 10 mmMatchWhat differs
      Property class 10.9InternationalISO 898-1≥ 940MPa1≥ 1 040MPa1—Reference grade.
      F3125 Grade A490United StatesASTM F3125/F3125M≥ 896MPa21 034–1 193MPa2Close match150–173 ksi (1034–1193 MPa) tensile, 130 ksi (896 MPa) yield; inch threads.