Matipedia

S350GD / Equivalents

Is it really S350GD? 2 “equivalents” checked

Cross-reference tables pair grades by name and history. Here each pairing is judged on the minimum values each standard guarantees, with the sources for both sides.

Close match

Same strength class; guaranteed values agree within a few MPa. Still check thickness bands and impact quality.

    Approximate

    Same class of steel, but at least one guaranteed value is lower or tested differently. Recheck the design.

    Not equivalent

    Commonly listed as an equivalent, but the guaranteed values do not support substitution.

      Side by side

      GradeStandardMin. yield at 10 mmTensile at 10 mmMatchWhat differs
      S350GDEuropeEN 10346:2015≥ 350MPa2≥ 420MPa2—Reference grade.
      A653 SS Grade 50 Class 1United StatesASTM A653/A653M≥ 340MPa2≥ 450MPa1ApproximateYield 340 MPa (50 ksi), 10 MPa lower; tensile 450 MPa (Class 1), higher. Elongation 12 % on 2 in., not comparable with A80.
      SGC490JapanJIS G 3302≥ 365MPa1≥ 490MPa1ApproximateHigher guaranteed yield (365 MPa) and tensile (490 MPa); listed as the JIS counterpart.