S460N
Normalized fine-grain steel: 460 MPa yield up to 16 mm, 540–720 MPa tensile up to 100 mm.
- Yield strength ReH
- ≥ 440MPaSingle source16–40 mm
- Tensile strength Rm
- 540–720MPaSingle source≤ 100 mm
- Elongation after fracture A
- ≥ 17%Single source
- Design yield strength fy
- 460MPaSingle source≤ 40 mm
- Design ultimate strength fu
- 540MPaSingle source≤ 40 mm
All values
Strength
Yield strength ReH
Upper yield strength guaranteed by the product standard (minimum).
| Condition | Value | Evidence |
|---|---|---|
| ≥ 460MPa | Single source | |
| ≥ 440MPa | Single source | |
| ≥ 430MPa | Single source | |
| ≥ 410MPa | Single source | |
| ≥ 400MPa | Single source | |
| ≥ 380MPa | Single source | |
| ≥ 370MPa | Single source |
Tensile strength Rm
Ultimate tensile strength. Product standards give a range or a minimum.
| Condition | Value | Evidence |
|---|---|---|
| 540–720MPa | Single source | |
| 530–710MPa | Single source |
Ductility
Elongation after fracture A
Minimum elongation; depends on gauge length and test direction.
| Condition | Value | Evidence |
|---|---|---|
| ≥ 17% | Single source |
Design values (Eurocode)
Design yield strength fy
Nominal value used in design calculations (before partial factors).
| Condition | Value | Evidence |
|---|---|---|
| 460MPa | Single source | |
| 430MPa | Single source |
Design ultimate strength fu
Nominal ultimate strength used in design calculations.
| Condition | Value | Evidence |
|---|---|---|
| 540MPa | Single source | |
| 540MPa | Single source |
Not yet verified for this grade
- A producer's datasheet for the product values
Missing on purpose: a value appears here only once a public source states it.
Sources here are public pages that reproduce EN 10025-3:2019. For design and acceptance, the standard edition named in your specification and the inspection certificate (EN 10204 3.1) of the delivered product take precedence.