SD345 vs A706 Grade 60
JIS G 3112 · Steel
Japanese deformed bar: yield 345–440 MPa, tensile ≥ 490 MPa, yield ratio ≤ 80 %.
ASTM A706/A706M · Steel
US low-alloy weldable rebar for seismic design: yield 60–78 ksi (420–540 MPa), tensile ≥ 80 ksi and ≥ 1.25 × actual yield.
Mechanical
| Property | Condition | SD345 | A706 Grade 60 | Difference |
|---|---|---|---|---|
| Yield strength ReH | — | 345–440MPa1 | 420–540MPa1 | +22 % |
| Tensile strength Rm | — | ≥ 490MPa1 | ≥ 550MPa1 | +12 % |
Rows are matched by condition (thickness band, temperature, product form). A dash means the grade has no sourced value for that condition. Differences are A706 Grade 60 relative to SD345; for ranges the lower bound is compared.