SD345 vs B500B
JIS G 3112 · Steel
Japanese deformed bar: yield 345–440 MPa, tensile ≥ 490 MPa, yield ratio ≤ 80 %.
BS 4449:2005+A3:2016 · Steel
Weldable rebar, ductility class B: 500 MPa characteristic yield, Rm/Re ≥ 1.08, Agt ≥ 5 %.
Mechanical
| Property | Condition | SD345 | B500B | Difference |
|---|---|---|---|---|
| Yield strength ReH | — | 345–440MPa1 | ≥ 500MPa1 | +45 % |
Rows are matched by condition (thickness band, temperature, product form). A dash means the grade has no sourced value for that condition. Differences are B500B relative to SD345; for ranges the lower bound is compared.