Matipedia

Compare / SD390 vs B500B

SD390 vs B500B

Japan JIS G 3112 · Steel

SD390

Japanese deformed bar: yield 390–510 MPa, tensile ≥ 560 MPa, yield ratio ≤ 80 %.

United Kingdom BS 4449:2005+A3:2016 · Steel

B500B

Weldable rebar, ductility class B: 500 MPa characteristic yield, Rm/Re ≥ 1.08, Agt ≥ 5 %.

Mechanical

PropertyConditionSD390B500BDifference
Yield strength ReH—390–510MPa1≥ 500MPa1+28 %

Rows are matched by condition (thickness band, temperature, product form). A dash means the grade has no sourced value for that condition. Differences are B500B relative to SD390; for ranges the lower bound is compared.