Matipedia
United StatesASTM A1085/A1085M· United States

A1085

US HSS with a yield cap: 50–70 ksi (345–483 MPa), 65 ksi (450 MPa) tensile, same for round and shaped.

Compared with S355J2H on its equivalents table.

All values

Strength

Yield strength ReH

ConditionValueEvidence
345–483MPaSingle source

Tensile strength Rm

ConditionValueEvidence
≥ 450MPaSingle source

Ductility

Elongation after fracture A

ConditionValueEvidence
≥ 21%Single source

Listed as equivalent to

  • S355J2H (EN 10219-1) — 345 MPa (50 ksi) yield with a 70 ksi cap, 450 MPa tensile, tighter wall tolerance; designed for seismic and full-thickness design.

Not yet verified for this grade

  • Charpy requirement and wall-thickness tolerance from a second source

Missing on purpose: a value appears here only once a public source states it.

Sources here are public pages that reproduce ASTM A1085/A1085M. For design and acceptance, the standard edition named in your specification and the inspection certificate (EN 10204 3.1) of the delivered product take precedence.