A500 Grade C
The usual US HSS grade: 50 ksi (345 MPa) yield shaped, 46 ksi (315 MPa) round, 62 ksi (425 MPa) tensile.
Compared with S355J2H on its equivalents table.
All values
Strength
Yield strength ReH
Upper yield strength guaranteed by the product standard (minimum).
| Condition | Value | Evidence |
|---|---|---|
| ≥ 345MPa | Corroborated | |
| ≥ 315MPa | Single source |
Tensile strength Rm
Ultimate tensile strength. Product standards give a range or a minimum.
| Condition | Value | Evidence |
|---|---|---|
| ≥ 425MPa | Corroborated |
Ductility
Elongation after fracture A
Minimum elongation; depends on gauge length and test direction.
| Condition | Value | Evidence |
|---|---|---|
| ≥ 21% | Corroborated |
Chemical composition
Show on the periodic tableA500 Grade C, heat analysis, % by mass, maximum
| Element | Applies to | Max % | Evidence |
|---|---|---|---|
| C | all thicknesses | 0.23 | Single source |
| Mn | all thicknesses | 1.35 | Single source |
| P | all thicknesses | 0.035 | Single source |
| S | all thicknesses | 0.035 | Single source |
Listed as equivalent to
- S355J2H (EN 10219-1) — Shaped A500 Grade C guarantees 345 MPa (50 ksi) and only 425 MPa tensile; round tubes only 315 MPa (46 ksi). No impact test.
Sources here are public pages that reproduce ASTM A500/A500M. For design and acceptance, the standard edition named in your specification and the inspection certificate (EN 10204 3.1) of the delivered product take precedence.