S275
Structural steel with 275 MPa minimum yield up to 16 mm, 410–560 MPa tensile.
S275JR1.004427 J at +20 °CS275J01.014327 J at 0 °CS275J21.014527 J at −20 °C
- Yield strength ReH
- ≥ 265MPaConfirmed16–40 mm
- Tensile strength Rm
- 410–560MPaConfirmed3–100 mm
All values
Strength
Yield strength ReH
Upper yield strength guaranteed by the product standard (minimum).
| Condition | Value | Evidence |
|---|---|---|
| ≥ 275MPa | Confirmed | |
| ≥ 265MPa | Confirmed | |
| ≥ 255MPa | Confirmed1 | |
| ≥ 245MPa | Confirmed | |
| ≥ 235MPa | Corroborated | |
| ≥ 225MPa | Corroborated | |
| ≥ 215MPa | Single source | |
| ≥ 205MPa | Single source |
Tensile strength Rm
Ultimate tensile strength. Product standards give a range or a minimum.
| Condition | Value | Evidence |
|---|---|---|
| 430–580MPa | Corroborated | |
| 410–560MPa | Confirmed1 | |
| 400–540MPa | Single source | |
| 380–540MPa | Single source |
S275 in other standards
Full comparison“Equivalent” tables online usually match grades by name. This one compares the values each standard actually guarantees, so a 30 MPa gap in yield is visible before it is in your calculation.
| Grade | Standard | Min. yield at 10 mm | Tensile at 10 mm | Match | What differs |
|---|---|---|---|---|---|
| S275 | ≥ 275MPa5 | 410–560MPa5 | — | Reference grade. | |
| 300W | ≥ 300MPa1 | 450–620MPa1 | Approximate | Yield 300 MPa (44 ksi), above S275; tensile 450–620 MPa. 44W is the imperial name. |
Not yet verified for this grade
- Elongation from a second source (Goldsupplier gives 23 %)
- Ladle analysis
Missing on purpose: a value appears here only once a public source states it.
Sources here are public pages that reproduce EN 10025-2:2019. For design and acceptance, the standard edition named in your specification and the inspection certificate (EN 10204 3.1) of the delivered product take precedence.