Standards
ASTM B265
ASTM B265
ASTM B265
Standard Specification for Titanium and Titanium Alloy Strip, Sheet, and Plate
Annealed titanium strip, sheet and plate by grade: unalloyed Grades 1–4, Ti-6Al-4V Grade 5 and others. Bars are covered by ASTM B348.
Official page4 values on this site name a clause of this document.
Grades on Matipedia
Titanium Grade 2
The workhorse unalloyed titanium: guaranteed Rp0.2 275 MPa, 4.51 g/cm³, outstanding resistance to seawater and chlorides.
- Rp0.2
- ≥ 275 MPa
- Rm
- 390–540 MPa
- Single source
- 14
- Trade sources only
- 2
- Disagreements explained
- 2
Ti-6Al-4V (Grade 5)
The most used titanium alloy: annealed Rm 895 MPa, Rp0.2 828 MPa at 4.4 g/cm³ — steel-like strength at 56 % of its weight.
- Rp0.2
- ≥ 828 MPa
- Rm
- ≥ 895 MPa
- Single source
- 19
- Disagreements explained
- 3