Matipedia

Compare / 500N (AS/NZS 4671) vs A706 Grade 60

500N (AS/NZS 4671) vs A706 Grade 60

Australia & New Zealand AS/NZS 4671 · Steel

500N (AS/NZS 4671)

Australian and New Zealand rebar: 500 MPa characteristic yield, normal ductility — Rm/Re ≥ 1.08, Agt ≥ 5 %.

United States ASTM A706/A706M · Steel

A706 Grade 60

US low-alloy weldable rebar for seismic design: yield 60–78 ksi (420–540 MPa), tensile ≥ 80 ksi and ≥ 1.25 × actual yield.

Mechanical

PropertyCondition500N (AS/NZS 4671)A706 Grade 60Difference
Yield strength ReH—500MPa1420–540MPa1
Tensile-to-yield ratio Rm/Re—≥ 1.081≥ 1.251+16 %

Rows are matched by condition (thickness band, temperature, product form). A dash means the grade has no sourced value for that condition. Differences are A706 Grade 60 relative to 500N (AS/NZS 4671); for ranges the lower bound is compared.