Matipedia

Compare / 500N (AS/NZS 4671) vs B500A

500N (AS/NZS 4671) vs B500A

Australia & New Zealand AS/NZS 4671 · Steel

500N (AS/NZS 4671)

Australian and New Zealand rebar: 500 MPa characteristic yield, normal ductility — Rm/Re ≥ 1.08, Agt ≥ 5 %.

United Kingdom BS 4449:2005+A3:2016 · Steel

B500A

Weldable rebar, ductility class A: 500 MPa characteristic yield, Rm/Re ≥ 1.05, Agt ≥ 2.5 %.

Mechanical

PropertyCondition500N (AS/NZS 4671)B500ADifference
Yield strength ReH—500MPa1≥ 500MPa2
Elongation at maximum force Agt—≥ 5%1≥ 2.5%3−50 %
Tensile-to-yield ratio Rm/Re—≥ 1.081≥ 1.053−2.8 %

Rows are matched by condition (thickness band, temperature, product form). A dash means the grade has no sourced value for that condition. Differences are B500A relative to 500N (AS/NZS 4671); for ranges the lower bound is compared.