Matipedia

Compare / 500N (AS/NZS 4671) vs B500B

500N (AS/NZS 4671) vs B500B

Australia & New Zealand AS/NZS 4671 · Steel

500N (AS/NZS 4671)

Australian and New Zealand rebar: 500 MPa characteristic yield, normal ductility — Rm/Re ≥ 1.08, Agt ≥ 5 %.

United Kingdom BS 4449:2005+A3:2016 · Steel

B500B

Weldable rebar, ductility class B: 500 MPa characteristic yield, Rm/Re ≥ 1.08, Agt ≥ 5 %.

Close matchSame 500 MPa, Rm/Re ≥ 1.08 and Agt ≥ 5 % as Eurocode class B; bar sizes and marking differ.

Mechanical

PropertyCondition500N (AS/NZS 4671)B500BDifference
Yield strength ReH—500MPa1≥ 500MPa1
Elongation at maximum force Agt—≥ 5%1≥ 5%2same
Tensile-to-yield ratio Rm/Re—≥ 1.081≥ 1.082same

Rows are matched by condition (thickness band, temperature, product form). A dash means the grade has no sourced value for that condition. Differences are B500B relative to 500N (AS/NZS 4671); for ranges the lower bound is compared.