Matipedia

Compare / 500N (AS/NZS 4671) vs B500C

500N (AS/NZS 4671) vs B500C

Australia & New Zealand AS/NZS 4671 · Steel

500N (AS/NZS 4671)

Australian and New Zealand rebar: 500 MPa characteristic yield, normal ductility — Rm/Re ≥ 1.08, Agt ≥ 5 %.

United Kingdom BS 4449:2005+A3:2016 · Steel

B500C

Weldable rebar, ductility class C: 500 MPa characteristic yield, Rm/Re ≥ 1.15 (< 1.35), Agt ≥ 7.5 %.

Mechanical

PropertyCondition500N (AS/NZS 4671)B500CDifference
Yield strength ReH—500MPa1≥ 500MPa1
Elongation at maximum force Agt—≥ 5%1≥ 7.5%2+50 %
Tensile-to-yield ratio Rm/Re—≥ 1.0811.15–1.352+6.5 %

Rows are matched by condition (thickness band, temperature, product form). A dash means the grade has no sourced value for that condition. Differences are B500C relative to 500N (AS/NZS 4671); for ranges the lower bound is compared.