Matipedia

Compare / Property class 8.8 vs F3125 Grade A325

Property class 8.8 vs F3125 Grade A325

International ISO 898-1 · Steel

Property class 8.8

The everyday structural bolt: 800 MPa tensile, 640 MPa yield (nominal). Minimums rise above 16 mm diameter.

United States ASTM F3125/F3125M · Steel

F3125 Grade A325

US heavy-hex structural bolt: 120 ksi (827 MPa) tensile, 92 ksi (634 MPa) yield. A325 now lives inside F3125.

Close match120 ksi (827 MPa) tensile and 92 ksi (634 MPa) yield, close to 8.8 above 16 mm; inch threads.

Mechanical

PropertyConditionProperty class 8.8F3125 Grade A325Difference
Elongation after fracture A—≥ 12%2≥ 14%1+17 %

Rows are matched by condition (thickness band, temperature, product form). A dash means the grade has no sourced value for that condition. Differences are F3125 Grade A325 relative to Property class 8.8; for ranges the lower bound is compared.