Matipedia

Compare / S350GD vs SGC490

S350GD vs SGC490

Europe EN 10346:2015 · Steel

S350GD

The most used steel for cold-formed purlins, light-gauge framing and decking: 350 MPa yield, 420 MPa tensile.

Japan JIS G 3302 · Steel

SGC490

Japanese hot-dip galvanized structural sheet: 365 MPa yield, 490 MPa tensile.

ApproximateHigher guaranteed yield (365 MPa) and tensile (490 MPa); listed as the JIS counterpart.

These two have no property in common yet. Open each page for its values.

Rows are matched by condition (thickness band, temperature, product form). A dash means the grade has no sourced value for that condition. Differences are SGC490 relative to S350GD; for ranges the lower bound is compared.