Japan JIS G 3112 · Steel

SD490

Japanese deformed bar: yield 490–625 MPa, tensile ≥ 620 MPa, yield ratio ≤ 80 %.

Australia & New Zealand AS/NZS 4671 · Steel

500N (AS/NZS 4671)

Australian and New Zealand rebar: 500 MPa characteristic yield, normal ductility — Rm/Re ≥ 1.08, Agt ≥ 5 %.

Mechanical

PropertyConditionSD490500N (AS/NZS 4671)Difference
Yield strength ReH—490–625MPa1500MPa1

Rows are matched by condition (thickness band, temperature, product form). A dash means the grade has no sourced value for that condition. Differences are 500N (AS/NZS 4671) relative to SD490; for ranges the lower bound is compared.