Compare / 500N (AS/NZS 4671) vs A615 Grade 60

500N (AS/NZS 4671) vs A615 Grade 60

Australia & New Zealand AS/NZS 4671 · Steel

500N (AS/NZS 4671)

Australian and New Zealand rebar: 500 MPa characteristic yield, normal ductility — Rm/Re ≥ 1.08, Agt ≥ 5 %.

United States ASTM A615/A615M · Steel

A615 Grade 60

The common US rebar: 60 ksi (420 MPa) yield. Not intended for welding; use A706 where welding or seismic ductility matters.

Mechanical

PropertyCondition500N (AS/NZS 4671)A615 Grade 60Difference
Yield strength ReH—500MPa1≥ 420MPa1

Rows are matched by condition (thickness band, temperature, product form). A dash means the grade has no sourced value for that condition. Differences are A615 Grade 60 relative to 500N (AS/NZS 4671); for ranges the lower bound is compared.