Matipedia

Compare / A615 Grade 60 vs 500N (AS/NZS 4671)

A615 Grade 60 vs 500N (AS/NZS 4671)

United States ASTM A615/A615M · Steel

A615 Grade 60

The common US rebar: 60 ksi (420 MPa) yield. Not intended for welding; use A706 where welding or seismic ductility matters.

Australia & New Zealand AS/NZS 4671 · Steel

500N (AS/NZS 4671)

Australian and New Zealand rebar: 500 MPa characteristic yield, normal ductility — Rm/Re ≥ 1.08, Agt ≥ 5 %.

Mechanical

PropertyConditionA615 Grade 60500N (AS/NZS 4671)Difference
Yield strength ReH—≥ 420MPa1500MPa1

Rows are matched by condition (thickness band, temperature, product form). A dash means the grade has no sourced value for that condition. Differences are 500N (AS/NZS 4671) relative to A615 Grade 60; for ranges the lower bound is compared.